Processing samples (Bi-Composite-Polishing Wheels)


Materials
NEW LAM M'MBlue / Green / Yellow
Diamond fluid
(grain size)
Roughness Ra μ

Tungsten carbide

25 μ / 10 μ

0,1 / 0,02
Silicon carbide
25 μ / 8 μ
0,15 / 0,05
Cobalt chrome alloy
10 μ / 6 μ
0,06 / 0,02
Treated Steel:
100CR6 / 210kg / 61 Rockwell C
25 μ / 8 μ / 6μ
0,15 / 0,015 / 0,008
Stainless Steel:
X30CR13
10 μ / 8 μ
0,12 / 0,035
Treated Stainless Steel
10 μ / 8 μ / 6 μ
0,06 / 0,03 / 0,012
Non-treated steel
15 μ / 10 μ / 6 μ
0,15 / 0,06 / 0,03
Cast-Iron CF25
25 μ / 10 μ
0,25 / 0,06
Bronze
8 μ
0,04
Ferrite
6 μ
0,09
Carbon
6 μ / 6 μ
0,15 / 0,10


General conditions of the trials:
Processing on a lappnig machine Ø 610 mm, wheel rotation speed: 60 rpm, surface area of pieces in contact to the wheel, per ring: 100 cm2, weight: 20 kg, pressure: 200 g/cm2 all values are standard values, no spezific values